拉制金属网
![]()
|
Type1) 型号 |
Mesh Ref No.2) 铁网型号 |
Material3) 材料 |
Nomial Size of Mesh 公称铁网尺寸 |
Thickness 厚度 (mm) |
Strand Width 网筋宽度 (mm) |
Weight 重量 KG / SHT ( ± 10% ) |
Standard Sheet Size 网片尺寸 SWM x LWM ( mm ) |
|
|
Short Way of Mesh SWM 铁网短距 ( mm ) |
Long Way of Mesh LWM 铁网长距 ( mm ) |
|||||||
|
Ornamesh or Lightmesh |
0515 0715 1015 1515 2015 |
Steel Steel Steel Steel Steel |
10 10 9 9 9 |
21 21 29 29 29 |
0.5 0.7 1.0 1.5 2.0 |
1.5 1.5 1.5 1.5 1.5 |
3.72 5.30 7.80 12.10 16.01 |
2400 x 1200 2400 x 1200 2400 x 1200 2400 x 1200 2400 x 1200 |
|
Security and Decorative Mesh |
1020 1520 1528 2028 2030 3035 3045 3060 4560 |
Steel Steel Steel Steel Steel Steel Steel Steel Steel |
16 16 22 22 35 22 35 42 42 |
38 38 57 57 76 57 76 115 115 |
1.0 1.5 1.5 2.0 2.0 3.0 3.0 3.0 4.5 |
2.0 2.0 2.8 2.8 3.0 3.5 4.5 6.0 6.0 |
5.41 9.19 8.29 11.00 7.49 21.00 19.01 23.90 35.71 |
2400 x 1200 2400 x 1200 2400 x 1200 2400 x 1200 2400 x 1200 2400 x 1200 2400 x 1200 2400 x 1200 2400 x 1200 |
|
Lourve Mesh |
1563 |
Steel |
16 |
76 |
1.5 |
6.3 |
29.95 |
2400 x 1200 |
|
Balustrage Mesh |
3032 |
Steel |
25 |
40 / 81 |
3.0 |
3.2 |
15.55 |
2400 x 1200 |
|
Walkway Mesh |
30080 50075 50080 50105 50110 |
Steel Steel Steel Steel Steel |
30 25 42 30 45 |
75 75 135 75 135 |
3.0 5.0 5.0 5.0 5.0 |
8.0 7.5 8.0 10.5 11.0 |
36.29 67.82 42.91 80.35 56.16 |
2400 x 1200 2400 x 1200 2400 x 1200 2400 x 1200 2400 x 1200 |
Notes : 1) All Metals can be flattened upon request. Suffice "F" to Mesh Ref. No. indicate flattened.
2) First 2 digits of Mesh Ref. No. indicate thickness ( thickness value x 10 ) and next 2 digits indicate
strand width ( strand width value x 10 ). In the case of walkway mesh, last 3 digits show strand
width ( strand width value x 10 ).
3) Expanded metal can be made from stainless steel (S304/316) or aluminium sheet (AA1100 - H14)
for Steel, it can be hot-dipped galvanised for corrosion resistance.